Nanoindentation

Material testing laboratory

Simulation Area

Move the mouse pointer on the images to see the details

Machine Over View

Protective Enclosure Indenter Head Berkovich Indenter Optical Microscope Sample Stage Sample

Observations

Test Parameters

Strain Rate 0.005 s⁻¹
Load Rate 0.2 mN/s
Displacement Rate 10 nm/s
Thermal Drift ≤ 0.05 nm/s
✖

Nano-Indentation Formulae

Contact Depth

hc = hmax − ε P S

hmax = maximum indentation depth, P = maximum load, S = unloading stiffness, ε ≈ 0.75 (Berkovich indenter)



Hardness Measurement

H = Pmax Ac

H = nanoindentation hardness, Pmax = maximum applied load, Ac = projected contact area


Elastic Modulus Determination

Er = 1 2β √(π / Ac) S

β = geometry correction factor (≈ 1.034 for Berkovich)


Specimen Modulus

1 Er = 1 − νs2 Es + 1 − νi2 Ei

Es, νs = modulus and Poisson’s ratio of the specimen,
Ei, νi = modulus and Poisson’s ratio of the indenter (for diamond: Ei ≈ 1140 GPa, νi ≈ 0.07)